| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 288 - 304 °C | 550 - 580 °F | |
|
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow
Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized
Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 30% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP1 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP4-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 210F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
|
|||
| Middle Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow
Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 288 - 304 °C | 550 - 580 °F | |
|
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Middle Barrel Temperature | 288 - 304 °C | 550 - 580 °F | |
|
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Middle Barrel Temperature | 288 - 304 °C | 550 - 580 °F | |
|
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Middle Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow
(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
LTL Color Compounds ColorFast® FRPC200 Polycarbonate, Flame-Retarded
Improved flame-retarded V0/5V injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||