Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
PTS SAN-82TR SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene
(discontinued **) Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Middle Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |