Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7336/GY7016 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8127 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8278/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8534 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8085/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7994 PEEK, unreinforced Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/40 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-0856/GY7 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-7720/BE PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 3 | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Zone 3 | 390 - 400 °C | 734 - 752 °F | |
Lehmann & Voss LUVOCOM® 1105-8344/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |