Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 25.0 °C | 77.0 °F | |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 55 AEX Thermoplastic Polyurethane Introduction: AVALON 55 AEX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 55 AEX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 60 DB Thermoplastic Polyurethane Introduction: AVALON 60 DB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DB is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 60 DE Thermoplastic Polyurethane Introduction: AVALON 60 DE is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 DE is part of the AVALON Perform Range and offers a premium soling materi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 98 AB Thermoplastic Polyurethane Introduction: AVALON 98 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 98 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Feed Temperature | 25.0 - 45.0 °C | 77.0 - 113 °F | Injection |
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 98 E 4066 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 98 E 4066 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 AC Thermoplastic Polyurethane Introduction: AVALON 65 AC is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 AC is part of the AVALON Crystal Range and offers a specially designed transparent materia.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 DB Thermoplastic Polyurethane Introduction: AVALON 65 DB is a polyester based thermoplastic polyurethane for injection molding. AVALON 65 DB is part of the AVALON Perform Range and offers a premium soling material for sports foo.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 65 DEU Thermoplastic Polyurethane Introduction: AVALON 65 DEU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 65 DEU is part of the AVALON Perform Range and offers a premi.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 70 ABX Thermoplastic Polyurethane Introduction: AVALON 70 ABX is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a speci.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 80 AB Thermoplastic Polyurethane Introduction: AVALON 75 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 75 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 ABX Thermoplastic Polyurethane Introduction: AVALON 85 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 90 ABR Thermoplastic Polyurethane Introduction: AVALON 90 ABR is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 90 ABR is part of the AVALON Performance Range and offers a premium soling .. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 92 AB Thermoplastic Polyurethane Introduction: AVALON 92 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 92 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 95 AB Thermoplastic Polyurethane Introduction: AVALON 95 AB is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 95 AB is part of the AVALON Performance Range and offers a premium soling ma.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 95 AE Thermoplastic Polyurethane Introduction: AVALON 95 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 95 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry Introduction: IROGRAN A 85 P 4854 is a flame-retardant, halogen-free polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4854 is part.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | Injection |
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 88 H 4622 TPU-Polyester Introduction: IROGRAN A 88 H 4622 is a black colored thermoplastic polyether/polyester-polyurethane for injection molding and extrusion applications. Additional characteristics of the product are hi.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4246 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 92 E 4246 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e.. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Feed Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Extrusion |
Huntsman IROGRAN® A 92 E 4738 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4738 is a white-colored, thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are flexibility and h.. |
|||
Feed Temperature | 25.0 - 35.0 °C | 77.0 - 95.0 °F | |
Huntsman AVALON® 85 ABU Thermoplastic Polyurethane Introduction: AVALON 85 ABU is a high performance UV-stabilized polyester based thermoplastic polyurethane for injection molding. AVALON 85 ABU is part of the AVALON Perform Range and offers a premi.. |