Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature 23.0 - 150 °C |
58.3 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® 6620U PBT+PC PBT+PC, Unfilled, Impact Modified, UV stabilized. Outstanding low temperature impact performance and chemical resistance. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Asia Pacific) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Asia Pacific) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East) General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Asia Pacific) Mold Release version of X7200This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East) Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X7300OQ PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. High flow with good impact and excellent optical quality.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -30.0 - 80.0 °C |
58.3 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
CTE, linear, Transverse to Flow | 105 µm/m-°C @Temperature -40.0 - 40.0 °C |
58.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent |