Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
0.950 g/cc
0.0343 lb/in³
ISO 1183
Moisture Absorption 0.0300 %
0.0300 %
50% RH, 24 hrs; ASTM D570
0.0300 %
0.0300 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm
<br>@Time 86400 sec
0.013 - 0.016 in/in
<br>@Time 24.0 hour
ASTM D955
0.0152 cm/cm
<br>@Time 86400 sec
0.0152 in/in
<br>@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0133 cm/cm
<br>@Time 86400 sec
0.0133 in/in
<br>@Time 24.0 hour
ISO 294
0.013 - 0.016 cm/cm
<br>@Time 86400 sec
0.013 - 0.016 in/in
<br>@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
21.0 MPa
3050 psi
ISO 527
Elongation at Break 47.6 %
47.6 %
ASTM D638
52 %
52 %
ISO 527
Elongation at Yield 6.2 %
6.2 %
ISO 527
8.4 %
8.4 %
ASTM D638
Tensile Modulus 1.22 GPa
177 ksi
1 mm/min; ISO 527
1.25 GPa
181 ksi
50 mm/min; ASTM D638
Flexural Strength 24.0 MPa
3480 psi
ISO 178
29.0 MPa
4210 psi
ASTM D790
Flexural Modulus 1.16 GPa
168 ksi
ISO 178
1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 8.17 J/cm
15.3 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D4812
Izod Impact, Notched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Dart Drop, Total Energy 33.0 J
24.3 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 32.0 J
23.6 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 102 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
56.7 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
102 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
56.7 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 105 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
105 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
58.3 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
51.0 °C
<br>@Thickness 3.20 mm
124 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved