Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 22.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 150 °C
12.2 µin/in-°F

@Temperature 32.0 - 302 °F
ASTM E831
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
12.2 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature >=143 °C
12.2 µin/in-°F

@Temperature >=289 °F
Above Tg; ISO 11359
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 90.0 °C
12.2 µin/in-°F

@Temperature 32.0 - 194 °F
2
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
2
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA), 16% Glass Fiber (Dry)
Amodel® AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
12.2 µin/in-°F

@Temperature -58.0 - 122 °F
1
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
12.2 µin/in-°F

@Temperature -58.0 - 122 °F
1
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 200 - 250 °C
12.2 µin/in-°F

@Temperature 392 - 482 °F
4
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 150 °C
12.2 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Noryl GTX GTX8721 PPE+PA
Noryl GTX GTX8721 resin is a glass and talc filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, conductivity, and low warpage. This ..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 90.0 °C
12.2 µin/in-°F

@Temperature 32.0 - 194 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 90.0 °C
12.2 µin/in-°F

@Temperature 32.0 - 194 °F
ASTM E831
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
12.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 0.000 - 100 °C
12.2 µin/in-°F

@Temperature 32.0 - 212 °F
TMA; ASTM E831
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry  (discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature >=143 °C
12.2 µin/in-°F

@Temperature >=289 °F
Above Tg; ASTM D696
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..
Copyright © lookpolymers.com All Rights Reserved