Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hour; ISO 306 |
Ineos ABS Lustran® Guardian™ 682 ABS, Injection Molding Grade Lustran® ABS 682 is a high performance, HCFC-141b resistant grade of ABS for injection molded refrigerator and freezer components. |
|||
Vicat Softening Point | 97.0 °C @Load 1.02 kg |
207 °F @Load 2.25 lb |
120°C/h; ASTM D 1525 |
Styrolution PS 165 N/L GPPS Styrolution PS 165N/L is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.High molecular weightGood flow characteristicsAppropriate for blending with HIPS.. |
|||
Vicat Softening Point | 97.0 °C @Load 1.02 kg |
207 °F @Load 2.25 lb |
50°C/h; ISO 306 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.10 kg |
207 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4026 Polypropylene Homopolymer, Film Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.10 kg |
207 °F @Load 11.2 lb |
50°C per hour; ISO 306 |
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.10 kg |
207 °F @Load 11.2 lb |
ISO 306 |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.10 kg |
207 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.10 kg |
207 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Bayblend® FR3000 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Easy-.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-716 ABS - High Flow High flow, medium impact |
|||
Vicat Softening Point | 97.0 °C @Load 1.00 kg |
207 °F @Load 2.20 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PG-22 Polystyrene TPE compound |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/min; ASTM D1525/B, ISO 306/B |
EPICHEM Epilac R ABS 10% GF Acrylonitrile Butadiene Styrene, 10% Glass Fiber Characteristics: 10% glass fibre filled |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-758R ABS - Transparent Transparent, Chemical Resistant |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PG-80 Polystyrene High strength |
|||
Vicat Softening Point | 97.0 °C @Load 1.00 kg |
207 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Chi Mei Polyrex® PG-80N Polystyrene High strength |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
120°C/hr; ISO 306 |
Chi Mei Polyrex® PG-80N Polystyrene High strength |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
50°C/hr; ISO 306 |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |