Thermal Properties Metric English Comments
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYblend 45FS GK25 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 5.001 kg
226 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYsan FL100 F35 SAN, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYabs F00 GF15 ABS, Glass Fiber-Reinforced
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 5.001 kg
226 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs H00 HF ABS, Heat Resistant, High Flow
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 5.001 kg
226 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYabs HF0 ABS
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 5.001 kg
226 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable
Information provided by Polykemi AB
Vicat Softening Point 108 °C

@Load 1.02 kg
226 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Styrolution PS 168 N/L GPPS
Styrolution PS 168N/L is a high molecular weight, heat resistant grade with high mechanical strength. It is suitable for physically or chemically expanded extruded sheet. It is also suitable for use..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution PS 168N GPPS
Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen..
Vicat Softening Point 108 °C

@Load 1.02 kg
226 °F

@Load 2.25 lb
120°C/h; ASTM D 1525
Styrolution PS 158 N/L GPPS
Styrolution PS 158N/L is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact polystyrene in heat contact applications; for..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ASTM D 1525
Styrolution PS 158K GPPS
Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper..
Vicat Softening Point 108 °C

@Load 5.00 kg
226 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0820 HT Acrylonitrile Butadiene Styrene
ABS with high thermal resistanceGood impact resistance, stiffness, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 108 °C

@Load 5.00 kg
226 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 108 °C

@Load 1.02 kg
226 °F

@Load 2.25 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9202 A Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 108 °C

@Load 1.02 kg
226 °F

@Load 2.25 lb
120°C/hr; ASTM D 1525
Cossa Polimeri ESTALUX 9202 Methyl Methacrylate Acrylonitrile Butadiene Styrene
Plastic blend that combines impact properties of ABS with the excellent transparency of PMMABiomedical grade in line with US pharmacopeia class VI USP and European pharmacopeia cap. 3.2.2Information..
Vicat Softening Point 108 °C

@Load 0.999 kg
226 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 2000 Styrene Acrylonitrile
General purpose SANGood chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 108 °C

@Load 0.999 kg
226 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTASAN SAN 3000 Styrene Acrylonitrile
High melt flow rate, good chemical resistance, excellent dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3006 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3010 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3010 IF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR3040 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3100 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® FR3110 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S..
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibilac® PW-997S ASA Polymer
Extrusion
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-106 L150 SAN
High Clarity
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-107 L125 SAN
High Clarity
Vicat Softening Point 108 °C

@Load 1.00 kg
226 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Polylac® PA-747R ABS - Extrusion
Attach case and refrigerator
Vicat Softening Point 108 °C

@Load 5.10 kg
226 °F

@Load 11.2 lb
120°C/h; ISO 306
Covestro Bayblend® FR630 GR PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Copyright © lookpolymers.com All Rights Reserved