Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 165 °C | 329 °F | Recommended |
Nye Lubricants 701 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20/XCF/35 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-0791 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7908 Polyphthalamide, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-7913 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8283 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Lehmann & Voss LUVOCOM® 20-8332 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP BMC 0160 is a general purpose BMC for electrical applications. Typical applications are lamp housings, canopies, covers and similar components.Information Provided by Menzolit |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0400 Unsaturated Polyester UP SMC 0400 is a Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to parts with good up to excellent surface quality for medium bake in-line and off-line p.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® BMC 2900 Unsaturated Polyester UP BMC 2900 is a specially designed BMC to meet the EC Safety Signs Directive (92/58/EEC) on the provision and use of safety signs at work. In areas where it is not possible to include the use of illu.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP SMC 0420 is a low density Premium Class-A SMC for exterior body applications on cars, LCV´s and trucks. These compounds mould to light weight parts with good up to excellent surface quality for .. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Maximum Service Temperature, Air | 165 °C @Time 10800 sec |
329 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6152 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 165 °C @Time 10800 sec |
329 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6153 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Maximum Service Temperature, Air | 165 °C @Time 10800 sec |
329 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6150 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 165 °C @Time 10800 sec |
329 °F @Time 3.00 hour |
no distortion |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® A3EG5 25% Glass Filled PA66 (Dry) Description: Glass fiber reinforced injection molding grade for machinery components and housings of high stiffness and dimensional stability such as coil formers and bearing cages. Also used for el.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5,000 hr |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | for 50% loss of tensile strength after 5000hr |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Maximum Service Temperature, Air | 165 °C | 329 °F | |
Atom Adhesives AA-DUCT 906 Epoxy Adhesive AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat.. |