Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer Menzolit
Trade Name Menzolit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is virtually nonburnable. In case of fire smoke is released to a small extent. Smoke is, except for carbon monoxyde non-toxic! This makes SMC 2400 very suitable for railway interior or exterior applications, like wall panels, window frames, luggage bins, seat shells and structures or similar rail way components. Fire safe furniture or sanitary furniture on ships, trains or prison cells are another typical use. Within the electrical industry it is used for arc quenching chambers or switch gear components that are exposed to high power switching operations and resulting electrical arcs (peak loads of temperature and fire).Information Provided by Menzolit
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Linear Mold Shrinkage 0.00080 cm/cm
0.00080 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.0 MPa

@Temperature 22.0 °C
8410 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Tensile Strength, Yield 58.0 MPa

@Temperature 22.0 °C
8410 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Modulus of Elasticity 9.00 GPa
1310 ksi
25mm flat samples, compression moulded; ISO 527-4
Flexural Strength 140 MPa

@Temperature 22.0 °C
20300 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 9.00 GPa

@Temperature 22.0 °C
1310 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
0.30
Shear Modulus 3.50 GPa
508 ksi
in plane
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C
>= 392 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 170 °C
338 °F
ISO 11357-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 70 %
70 %
ISO 4589-2
Glow Wire Test 960 °C
1760 °F
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 24.0 kV/mm
610 kV/in
IEC 60243-1
Dissipation Factor 0.010
0.010
IEC 60250
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 150 °C
275 - 302 °F
Compression moulding, matched metal die