Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 100 °C | 212 °F | Recommended |
Nye Lubricants 731W Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Recommended |
Nye Lubricants 751B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Recommended |
Nye Lubricants 757SSG (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Maximum operating temperature continuously for 5000 hours based on a tensile stress of 50% at 23° C. |
Omnia Plastica Akulon® POM h Acetal Homopolymer The general features of homopolymer acetalic resin are similar to those of copolymer POM c, except that service temperature (under load) is slightly higher but resistance to hydrolysis and strong al.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Precision Polymer Engineering Q70R Polyurethane Rubber Peroxide cured, red Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion r.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Precision Polymer Engineering R70D Natural Rubber Natural Rubber, 65-75 °IRHD. Formulated to Defence Standard 93-30, Type QX, Grade 70 (NRQX70).Applications: Natural rubber offers low compression set, high tensile strength, high resilience and ex.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous; FRISETTA Test Method |
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-7489 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Retains Stretch |
Freudenberg Simrit 92 AU 21100 Low Temperature Polyurethane Elastomer With the new low temperature material 92 AU 21100, Simrit has succeeded in developing a polyurethane material that is specially designed to meet the specific requirements for use at low temperatures.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
GEHR Plastics POM-10PE Acetal Copolymer Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® 80-8072 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30 PA666-GF30 Product description: Grilon TSG-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers. Grilon TSG-30 has the following important properties: Excellent fl.. |
|||
Maximum Service Temperature, Air | 100 - 130 °C | 212 - 266 °F | long term; EMS |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-35 PA666-GF35 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 - 120 °C | 212 - 248 °F | long term; EMS |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | Continuous; UL746B |
Ensinger Tecaform™ AH ID Metal Detectable Acetal Copolymer (POM) TECAFORM™ AH ID is the fist commercially available acetal that is fully detectable by standard metal detection equipment. Exhibiting excellent machinability and a good combination of physical prop.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | ASTM D 3575 |
Eurofoam Porocell POR 303/B RS CR-Neoprene/NBR Foam Polychloroprene and acrylonitrile butadiene foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Azoty Tarnow™ TARNOFORM 400 POM Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
Azoty Tarnow™ TARNOFORM 500 UV POM High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
BASF Ultraform® S1320 003 POM Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat.. |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Maximum Service Temperature, Air | 100 °C | 212 °F | long term; EMS |
EMS-Grivory Grivory® TS FR PA666 FR Information provided by EMS Grivory |