Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Recommended |
Nye Lubricants 759X (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Short Term Use |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
Nilit Nilamon A3 H K8 40% Mineral Reinforced PA66 Description: Nilamon A3 H K8 combines good stiffness with low warpage. It is used for applications which need a degree of rigidity, particularly at higher temperatures, but which need to stay flat a.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FORM 5526 EMI Shielding Material Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 4076 Conductive Coating CHO-SHIELD® 4076 nickel-filled polyurethane is recommended for shielding an entire room. This durable coating adheres well to plaster, wood, glass, concrete, drywall and most metals.Information pro.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 4994 Conductive Flexible Coating Description: CHO-SHIELD® 4994 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesi.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous (GTP 50% Tensile); IEC 60216 |
PolyOne Bergamid™ B700 UF black Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 20,000 hr; IEC 216 |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FLEX 4430 Conductive Ink CHO-FLEX polyester inks were developed for the membrane keyboard and sensor industries. The ink bond to Mylar films, and can be creased, heat-formed or scratched without affecting their performance... |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FLEX 4432 Conductive Ink CHO-FLEX polyester inks were developed for the membrane keyboard and sensor industries. The ink bond to Mylar films, and can be creased, heat-formed or scratched without affecting their performance... |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; 5,000 h |
Quadrant EPP Nylatron® MD PA 6 + metal detectable additive, extruded (ISO Data) Metal detectable 6SA grade High wear and fatigue resistance Lower moisture absorption than standard PA6 Metal and visual detection by blue colour Detection by x-ray also possible Continuous use temp.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; DIN 52612 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Heat Distortion Temp |
Hannam Chemical Hanalac 780 ABS, High Flow FDA Approved. High flow grade suitable for intricate or thin structures and low processing cycle time. Applications include TVs, radios, calculators, appliances, toys. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
LATI Latamid 6 BH PA 6, Heat Stabilized Polyamide 6 (PA6). High fluidity. Heat stabilized. Very high fluidity.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R491 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R496 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R650 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Trelleborg R520 Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | Continuous; UL746B |
Ensinger Delrin® 150 Homopolymer Acetal (POM) Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | 5000 h; VDE 0304/P2-1, IEC 216 |
EPICHEM PA 66 Polyamide 66 |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-FORM 5531 EMI Shielding Material One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. It is designed.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Maximum Service Temperature, Air | 85.0 °C | 185 °F | |
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding.. |
|||
Maximum Service Temperature, Air | 85.0 - 190 °C | 185 - 374 °F | Average value: 147 °C Grade Count:14 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |