Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding performance. CHO-SHIELD® 2040’s robust formulation can be applied in both high and low volume paint application. CHO-SHIELD® 2040 is ideal for use on electronic enclosures and assemblies. CHO-SHIELD® 2040’s composition allows for simple, standard application using conventional equipment with minimal dry-time and handling. CHO-SHIELD® 2040 is ideal for use on medical electronic enclosures and assemblies which require high level, reliable EMI shielding performance and may benefit from silver’s antimicrobial properties.Application: Superior EMI shielding, Anti-static protection, Surface grounding, Coating of ABS, PC/ABS, and many other types of plastic enclosures.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.10 - 1.50 g/cc
1.10 - 1.50 g/cc
ASTM D792
Solids Content 42 %
42 %
Volatile Organic Compounds (VOC) Content 741 g/l
741 g/l
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 85.0 °C
185 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.025 ohm

@Thickness 0.0250 mm
<= 0.025 ohm

@Thickness 0.000984 in
Shielding Effectiveness 73 dB

@Frequency 1.00e+10 Hz
73 dB

@Frequency 1.00e+10 Hz
>= 75 dB

@Frequency 10000 - 8.00e+7 Hz
>= 75 dB

@Frequency 10000 - 8.00e+7 Hz
80 dB

@Frequency 1.00e+8 Hz
80 dB

@Frequency 1.00e+8 Hz
85 dB

@Frequency 1.00e+9 Hz
85 dB

@Frequency 1.00e+9 Hz
Processing Properties Metric English Comments
Dry Time 0.500 hour

@Temperature 24.0 °C
0.500 hour

@Temperature 75.2 °F
Tack Free
10 - 20.0 hour

@Temperature 24.0 °C
10 - 20.0 hour

@Temperature 75.2 °F
then 30 minutes at 65°C
24.0 hour

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Full Dry
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesion 5B
ASTM D 3359
Coverage 267 sq ft/gal
at 0.001 in
Filler Silver
Polymer Acrylic
Suggested Spraying Viscosity #2 Zahn Cup 16 - 22 sec