Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
±0.03 g/cm³; DIN 53479
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa

@Temperature 23.0 °C
7980 psi

@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 20 %

@Temperature 23.0 °C
20 %

@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 1.50 GPa

@Temperature 23.0 °C
218 ksi

@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.630 J/cm²

@Temperature -30.0 °C
3.00 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
0.840 J/cm²

@Temperature 23.0 °C
4.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
ISO 3146
Maximum Service Temperature, Air 85.0 °C
185 °F
Continuous (GTP 50% Tensile); IEC 60216
160 °C
320 °F
Short Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Unannealed; ISO 75-2/A
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
ALL; Internal Method
Glow Wire Test 960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Constant 7.0

@Frequency 1.00e+6 Hz
7.0

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 45.0 kV/mm
1140 kV/in
IEC 60243-1
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Descriptive Properties Value Comments
Features Flame Retardant
Halogen Free
Low (to None) Phosphorus Content
Forms Pellets
Generic Material Nylon 6
Generic Name Polyamide 6 (Nylon 6)
K-Value 74.0 to 78.0
No Standard; 96% H2SO4
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: