Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | >= 240 °C | >= 464 °F | UL RTI |
Rogers Corporation Ultralam® 3908 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3908 bondply is used as a bonding medium between copper and the dielectric material. This product was developed specifically for multi-layer substrate constructions. This adhesiveless f.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Heat distortion temperature, load unknown; ASTM D648 |
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-7294/BL PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber The linear polyphenylensulfide belongs to the semi-crystalline materials and offers a very high mechanical capacity, thermal and chemical resistance distinguished at the same time, high dimensional .. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
Greene Tweed CHEMRAZ® 592 Perfluoroelastomer Chemraz® 592, a versatile perfluoroelastomer developed with a proprietary filler system, is very resistant to plasma attack. This compound’s durometer allows for some hardware finish incons.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-0915 PPS, linear, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term |
Lehmann & Voss LUVOCOM® 1301-7767 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short peaks operation |
Polyram PlusTek PA301G2 Nylon 6.6 for Injection Molding, 10% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 10% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short peaks operation |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short peaks operation |
Polyram PlusTek PA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, flame retardant, halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short peaks operation |
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction 30% Glass fiber reinforced Nylon 66 for low friction applications.Information provided by Polyram. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short peaks operation |
Polyram PlusTek RA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, self extinguishing halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Continuous |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
Unitika TERRAMAC TE-1070 Polylactic Acid (PLA) High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
Unitika TERRAMAC TE-2000 Polylactic Acid (PLA) Basic grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term; EMS |
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30 Grivory TH2V-3H LF is a glass fiber reinforced (30%), PTFE modified engineering thermoplastic based on semi-crystalline partially aromatic copolyamide. Polymer designation acc. ISO: PA6T/66 Polymer .. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term; EMS |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term; EMS |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | short term; EMS |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | Short term |
CENTROPLAST CENTROTRON GF 15 Polyphenylene sulfide 15% glass fiber CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used in high temperature applications. CENTROTRON has a low sliding friction coefficient and high abrasion resista.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
3M Dyneon™ PFA FLEX 8502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon™ PFA-FLEX UHP family exhibits improved environmental stress crack resistance to stress cracking agents such as fluorsurfactants and fluorosurfactant-containing chemicals. In addition, this f.. |
|||
Maximum Service Temperature, Air | 240 °C | 464 °F | |
3M Dyneon™ PFA FLEX 8515 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon™ PFA-FLEX UHP family exhibits improved environmental stress crack resistance to stress cracking agents such as fluorsurfactants and fluorosurfactant-containing chemicals. In addition, this f.. |