| Category | Polymer , Thermoplastic |
| Manufacturer | Wolf Kunststoff |
| Trade Name | ZEDEX® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.06 g/cc | 0.0744 lb/in³ | ISO 1183 |
| Water Absorption | 0.010 % <br>@Temperature 23.0 °C |
0.010 % <br>@Temperature 73.4 °F |
RMC 93%; DIN EN ISO 62 |
| Moisture Absorption at Equilibrium | 0.020 % | 0.020 % | DIN EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 100 | >= 100 | DIN 53505 |
| Hardness, Shore D | 65 | 65 | DIN 53505 |
| Ball Indentation Hardness | 36.0 MPa | 5220 psi | DIN 2039 |
| Tensile Strength at Break | 10.8 MPa | 1570 psi | DIN EN ISO 527 |
| Tensile Strength | 12.7 MPa | 1840 psi | DIN EN ISO 527 |
| Tensile Stress | 0.800 MPa <br>@Strain 1.00 %,<br> Time 3.60e+6 sec |
116 psi <br>@Strain 1.00 %,<br> Time 1000 hour |
DIN 53444 |
| Tensile Strength, Yield | 9.80 MPa | 1420 psi | Elastic Limit |
| 12.7 MPa | 1840 psi | DIN EN ISO 527 | |
| Elongation at Break | 92 % | 92 % | |
| 92 % | 92 % | DIN EN ISO 527 | |
| Elongation at Yield | 1.3 % | 1.3 % | Elastic Yield Point |
| 2.3 % | 2.3 % | Elongation at Maximum Force; DIN EN ISO 527 | |
| 2.3 % | 2.3 % | DIN EN ISO 527 | |
| 4.2 % | 4.2 % | Flexural; DIN EN ISO 178 | |
| Tensile Modulus | 0.800 GPa | 116 ksi | DIN EN ISO 527 |
| Flexural Strength | 18.9 MPa | 2740 psi | DIN EN ISO 178 |
| 19.0 MPa | 2760 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 | |
| Flexural Modulus | 1.17 GPa | 170 ksi | DIN EN ISO 178 |
| Compressive Strength | 16.0 MPa | 2320 psi | Elastic Limit |
| 1.00 MPa <br>@Time 3.60e+7 sec |
145 psi <br>@Time 10000 hour |
||
| 12.0 MPa <br>@Time 360000 sec |
1740 psi <br>@Time 100 hour |
||
| 15.0 MPa <br>@Time 36.0 sec |
2180 psi <br>@Time 0.0100 hour |
||
| 16.0 MPa <br>@Strain 3.50 % |
2320 psi <br>@Strain 3.50 % |
DIN EN ISO 604 | |
| Compressive Modulus | 1.49 GPa | 216 ksi | DIN EN ISO 604 |
| Fatigue Strength | 7.00 MPa <br>@# of Cycles 1.00e+6 |
1020 psi <br>@# of Cycles 1.00e+6 |
1 Hz |
| K Factor (ISO) | 0.50 µm/km <br>@Temperature 20.0 °C |
0.50 µm/km <br>@Temperature 68.0 °F |
|
| 0.60 µm/km <br>@Temperature 100 °C |
0.60 µm/km <br>@Temperature 212 °F |
||
| 4.9 µm/km <br>@Temperature 200 °C |
4.9 µm/km <br>@Temperature 392 °F |
||
| 5.6 µm/km <br>@Temperature 240 °C |
5.6 µm/km <br>@Temperature 464 °F |
||
| Charpy Impact Unnotched | NB | NB | EN ISO 179/1eU |
| Charpy Impact, Notched | 12.3 J/cm² | 58.5 ft-lb/in² | EN ISO 179/1eA |
| Coefficient of Friction, Dynamic | 0.070 <br>@Temperature 100 °C |
0.070 <br>@Temperature 212 °F |
Dry Operation |
| 0.11 <br>@Temperature 20.0 °C |
0.11 <br>@Temperature 68.0 °F |
Dry Operation | |
| Coefficient of Friction, Static | 0.12 <br>@Temperature 20.0 °C |
0.12 <br>@Temperature 68.0 °F |
Dry Operation |
| Tensile Creep Modulus, 1000 hours | 60.0 MPa | 8700 psi | At 1% Deformation; DIN 53444 |
| Limiting Pressure Velocity | 0.0347 MPa-m/sec | 991 psi-ft/min | v = 1m/min |
| 0.233 MPa-m/sec | 6650 psi-ft/min | v = 200m/min | |
| 0.285 MPa-m/sec | 8140 psi-ft/min | v = 10m/min | |
| 0.3167 MPa-m/sec | 9042 psi-ft/min | v = 100m/min | |
| Compression Set | 3.5 % | 3.5 % | Elastic Compression Limit |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 120 µm/m-°C <br>@Temperature <=100 °C |
66.7 µin/in-°F <br>@Temperature <=212 °F |
ISO E 830 |
| 160 µm/m-°C <br>@Temperature <=150 °C |
88.9 µin/in-°F <br>@Temperature <=302 °F |
ISO E 831 | |
| Specific Heat Capacity | 0.760 J/g-°C | 0.182 BTU/lb-°F | DSC |
| Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 327 °C | 621 °F | DSC |
| Maximum Service Temperature, Air | 240 °C | 464 °F | Continuous |
| 260 °C | 500 °F | Short Term (3h) | |
| Glass Transition Temp, Tg | -20.0 °C | -4.00 °F | DSC |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 95 % | 95 % | DIN EN ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+19 ohm-cm | 1.00e+19 ohm-cm | IEC 93 |
| Surface Resistance | 5.50e+12 ohm | 5.50e+12 ohm | IEC 93 |
| Dielectric Constant | 2.7 <br>@Frequency 110 Hz |
2.7 <br>@Frequency 110 Hz |
IEC 250 |
| Dielectric Strength | 14.0 kV/mm | 356 kV/in | IEC 243 |
| Dissipation Factor | 0.00030 | 0.00030 | IEC 112 |
| 0.103 <br>@Frequency 1.00 Hz |
0.103 <br>@Frequency 1.00 Hz |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Alignment Adjustment | 2 | Nominal Scale: 1, low; 10, high |
| Chemical Sterilization | 10 | Nominal Scale: 1, low; 10, high |
| Color | Brown | |
| Creep Resistance | 1 | Nominal Scale: 1, low; 10, high |
| Dimensional Stability with Thermal Expansion | 1 | Nominal Scale: 1, low; 10, high |
| Free from Silicon | Applicable | |
| High Precision Bushings (negative clearance) | Applicable | |
| Injection Molded Parts | Applicable | |
| Machined Parts | Applicable | |
| Moist Heat Sterilization | 10 | Nominal Scale: 1, low; 10, high |
| Plastic Granules | Applicable | |
| Resistance Against dust, Dirt, Abrasive Substances | 2 | Nominal Scale: 1, low; 10, high |
| Resistance Against Hot Water | 250 | |
| Resistance to Chemicals | 10 | Nominal Scale: 1, low; 10, high |
| Resistant Against Disinfectant | Applicable | |
| Rods up to Øe (de) | Applicable | |
| ROHS/WEEE | Applicable | |
| Sheets up to Maximum Thickness | Applicable | |
| Sliding Velocity | 250 | |
| Suitable for Outdoor Use | 10 | Nominal Scale: 1, low; 10, high |
| Suitable for Use in Water | Applicable | |
| Suitable for Vacuum | Applicable | |
| Tubes (hollow rods) up to Øe (de) | Applicable | |
| UV Rays Resistance | 9 | Nominal Scale: 1, low; 10, high |