Polymer Property : Decomposition Temperature = 572 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 300 °C
572 °F
1% mass loss, N2; TGA
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® 1C PA6/66 (Dry)
Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® A24 E 01 PA66
Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3EG6 LS BK 23189 30% Glass Filled PA6 (Conditioned)
Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B40 L PA6
Description: Ultramid® B40 L is a lubricated polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round ..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B40 PA6
Description: Ultramid® B40 is a polyamide 6 grade of high viscosity that is well suited for the production of blown and cast film and monofilaments. Product supplied in 2-2.5 mm round pellets.Infor..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® C31 01 PA6/66
Description: Ultramid® C31 01 is a copolyamide 6/66 grade of low viscosity that is well suited for the production of compounds and blends. Product supplied in 2-2.5 mm CYLINDRICAL pellets.Informati..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® C40 L 01 PA6/66
Description: Ultramid® C40 L 01 is a lubricated copolyamide 6/66 grade of high viscosity for the production of monofilaments and blown film. Ultramid® C40 L 01 is well suited for the production of..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B27 SD 02 PA6
Description: Ultramid® B27 SD 02 is a polyamide 6 for the production of semi dull textile and carpet fibers. Product comes in 2-2.5 mm cylindrical pellets.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B33 L PA6
Description: Ultramid® B33 L is a lubricated polyamide 6 grade of intermediate viscosity that is well suited for the production of biaxial oriented and cast film and monofilaments. Product comes ..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B33 LV PA6
Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B35G3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass fiber reinforced injection molding grade e.g. for internal gas pressure applications such as flashing direction switch gears, automobile mirror housings and wheels of mountain..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B36 LN 0.04 mm Cast Film Cold Chillroll
Product comes in 2-2.5 mm round pellets.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Conditioned)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Conditioned)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG6 HP BK 23210 30% Glass Filled PA6 (Dry)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade with enhances flowability used e.g. for automobile manifold.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3UG4 LS BK 23215 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3UG4 LS Grey 22985 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Conditioned)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG10 BK 00564 50% Glass Filled PA6 (Dry)
Description: 50% glass-fiber reinforced and heat aging resistant injection-molding grade for technical parts with very high stiffness.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry)
Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® Seal-Fit PA6/66 (Conditioned)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..
Decomposition Temperature >= 300 °C
>= 572 °F
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..