Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 3.20 mm |
302 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Ovation Polymers OpteSTAT™ NC PK 8010 Polyetheretherketone based Carbon Nanotube Compound Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Lexan® PPC4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ISO 75 |
Gharda Chemicals GATONE™ 5300 PEEK, High Viscosity Grade
(discontinued **) High viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical propert.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ISO 75 |
Gharda Chemicals GATONE™ 5400 PEEK, Medium Viscosity Grade
(discontinued **) Medium viscosity grade for extrusion and injection moldingCHARACTERISTICS: Outstanding chemical resistance.Outstanding wear resistance.Outstanding resistance to hydrolysis.Excellent mechanical prope.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | |
Covestro Apec® 1700 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 3.17 mm |
302 °F @Thickness 0.125 in |
ASTM D648 |
Covestro Apec® DP9-9340R High-Heat Polycarbonate, Medical with Release
(discontinued **) It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 3.17 mm |
302 °F @Thickness 0.125 in |
ASTM D648 |
Covestro Apec® DP9-9341 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 - 250 °C | 302 - 482 °F | Average value: 180 °C Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 150 °C | >= 302 °F | ISO 75-2 |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 150 °C | >= 302 °F | ISO 75-2 |
Menzolit Menzolit® BMC 1650 Unsaturated Polyester UP BMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 150 °C | >= 302 °F | ISO 75-2 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 3.20 mm |
302 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 6.40 mm |
302 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® VB-3100G PBT/ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ISO 75-93 |
Wellman Wellamid® MR410 42H-NBK1 40% Mineral Reinforced Nylon 6 Description: Mineral Reinforced Nylon 6Information provided by Wellman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | 120°C/hr; ASTM D 648 |
Cossa Polimeri ESTAPROP H 0580 GFC Polypropylene, 40% Glass Filled PP homopolymer 40% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ISO 75-1/-2 |
DuPont Performance Polymers Crastin® LW9020 BK580 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 BK580 is a 20% glass fiber reinforced black polybutylene terephthalate blend for injection mol.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
Eurostar Staramide AK8ST41 PA66, Mineral Reinforced, Impact Modified, Injection Molding Staramide AK8ST41 is an Impact Modified, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339G10CL Glass Reinforced Coupled |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ISO 75-1/-2 |
Barlog Plastics KEBAPEAK XS1700 PEEK, unreinforced PEEKInformation provided by BARLOG plastics GmbH. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ASTM D648 |
Asahi Kasei Thermylene® P6-40FM-2371 40% Glass Fiber/Mica Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C | 302 °F | 80*10*4mm, Cut; ISO 75-1&2 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 °C @Thickness 3.20 mm |
302 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3230A PP SABIC® PPcompound G3230A is a general purpose, 30% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS ID is 109612410 |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 150 - 170 °C | 302 - 338 °F | ISO 75 Af |
Vyncolit 3520 CG Novolac Phenolic Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par.. |