Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 178 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycolac® MG29 ABS
Super high impact ABS. Good low temperature toughness. High gloss.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D648
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East)
CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped..
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
0.125 in bar, Unannealed/Conditioned 48 hours; ASTM D648
Network Polymers NPP 808 C3WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Annealed; ASTM D648
Network Polymers NPS 90-0802 Polystyrene
Description: Injection Molding Grade, High ImpactInformation provided by Network Polymers Inc.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific)
Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1...
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Resirene Resirene® 6420 Super High Impact Polystyrene
Features:Super High ImpactEasy ProcessingLow ModulusFlexibilityFDA Rating: 21 CFR 177.1640Applications:ExtrusionDeep ThermoformingGPPS/HIPS BlendsPoint of Purchase DisplaysInformation provided by US..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Resirene Resirene® 9720 High Impact Polystyrene
Features:Medium FlowHigh Thermal ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingInjectionDisposablesGPPS/HIPS BlendsInformation provided by US distributor..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
120°C/h; ISO 75/1
Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Unannealed; ISO 75-2A
Total Lacqrene® 1250 Crystal Polystyrene  (discontinued **)
LACQRENE® 1250 is a very high molecular weight crystal polystyrene mainly for the injection molding industry. It is characterized by a very good compromise between molecular weight, heat resistanc..
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
ASTM D648
I. Stern 550 High Impact Polystyrene
Features:Good process propertiesExcellent toughness and environmental stress crackingApplicationsStructural foamDisplaysSmall appliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Informat..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
LG Chemical HI855H PMMA, Impact Resistant Grade
Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 12.7 mm
178 °F

@Thickness 0.500 in
Unannealed; ASTM D648
LG Chemical SI-610 Alphalac Polystyrene
High flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include big size electric app..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP KP004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP004L is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C

@Thickness 6.40 mm
178 °F

@Thickness 0.252 in
ASTM D648
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER
PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SP 556 Flame Retardant Polystyrene
Characteristics Good flow properties Good balance of toughness and rigidity Available in any color Processing Extrusion MoldingApplications T.V. Cabinets, computer monitor, printer housing Elect..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SP 562 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Eastman Tritan LX150HF Copolyester
Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades ..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Unannealed; ASTM Data
Dow Tyril® 1011 SAN
TYRIL® 1011 SAN copolymer is a light stabilized general purpose injection molding resin available in crystone color only. It exhibits excellent weathering characteristics, high strength, good chemi..
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
Aclo Accutech Polypropylene Homopolymer HP0336M40L Mica Reinforced
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °C
178 °F
ASTM D648
Americas Styrenics STYRON® 487 High Impact Polystyrene
Product CharacteristicsGood TrimmabilityToughnessHeat resistanceFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by A..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM Data
BASF Capron® 5202CQ Blend HS Blend Nylon 66 (Dry)  (discontinued **)
Capron 5202CQ HS Blend is a heat stabilized, blended polyamide 6,6 injection molding homopolymer developed for fast molding cycles. It is also available in pigmented versions.Capron 5202CQ HS Blend..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
annealed; ASTM D648
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
ASTM D648
Supreme Petrochem SP 731 9920 High Impact Polystyrene
Characteristics Speciality grade containing silicon oil to provide wear resistance and high opacity jet black color Easy flowing grade Processing Injection moldingApplications Camera parts Photogr..
Deflection Temperature at 1.8 MPa (264 psi) 81.0 - 216 °C
178 - 421 °F
Average value: 191 °C Grade Count:13
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..