Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648-95 |
Multibase Multi-Pro® 2005 M 20% Mica Filled Polypropylene Multi-Pro 2005 M is a mica reinforced polypropylene compound with high stiffness and flex strength. Its high heat resistance lends itself to replace engineered plastics at moderate cost.Data provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs S20 ABS Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 3.20 mm |
171 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Treatment Temp. 60.0 °C |
171 °F @Treatment Temp. 140 °F |
Annealed; ASTM D648 |
PolyOne Geon™ L6105 natural Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 3.20 mm |
171 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS (Asia Pacific) LNP* Lubricomp* CBL36XXC is a compound based on Polystyrene resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 6.40 mm |
171 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS 405AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 3.20 mm |
171 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 3.20 mm |
171 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® IQNH2900 PBT+PC Import Grade. UL94 V-0 Performance with Non-Brominated Flame Retardant. PCR% is up to 12% by using Valox iQ* resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C @Thickness 6.40 mm |
171 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® TF-0959 T HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Unannealed; ASTM Data |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Annealed; ASTM D648 |
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer DescriptionPolyfort® FPP 1603 is a 10% glass reinforced copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer DescriptionPolyfort® FPP 1603 is a 10% glass reinforced copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer DescriptionPolyfort® FPP 1603 is a 10% glass reinforced copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 3502E Description: Extrusion Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | 0.125";; ASTM D648 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
Diamond Polymers NYLON 6630 L Black Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
Clariant Renol PA113 Nylon 66, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | 0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648 |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | |
Aclo Accutech Polypropylene Homopolymer HP0339W30L1 Wollastonite Reinforced |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | ASTM D648 |
Chem Polymer Chemlon 102 Nylon 66, Nucleated A highly nucleated, lubricated nylon 66 intended for fast cycling applications. Increased tensile strength, rigidity, creep resistance and hardness over general purpose 66.Data provided by the manu.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D648 |
Eastman Tenite Acetate 109E3V46022 Natural, Trsp Cellulose Acetate
(discontinued **) Plasticizer 25%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.2% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 77.0 °C | 171 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |