Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Molded, Unreinforced
Manufacturer Americas Styrenics LLC
Trade Name STYRON™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™ 668 complies with U.S. FDA 21 CFR 177.1640.Information provided by DowAmericas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 5.3 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.3 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.0 MPa
7400 psi
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Tensile Strength, Yield 51.0 MPa
7400 psi
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Tensile Modulus 3.134 GPa
454.5 ksi
0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Flexural Strength 102 MPa
14800 psi
0.05 in/min; 3-point; ASTM D790
Flexural Modulus 3.54 GPa
513 ksi
0.05 in/min; 3-point; ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
0.5 x 0.125 in.; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C
192 °F
unannealed; injection molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.2 °C
171 °F
unannealed; injection molded; ASTM D648
Vicat Softening Point 105 °C
221 °F
120°C/hr, 1 kg; ASTM D1525-B
Flammability, UL94 HB
HB
0.06 in. thickness
Optical Properties Metric English Comments
Refractive Index 1.59
1.59
ASTM D542
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003
Users viewing this material also viewed the following: