Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | |
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPC K20040 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ISO 75-2/A |
PolyOne Bergamid™ B70 UF V2 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Halar® 5001C Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)& Powder grades for masterbatches.Information provided by Solvay Specialty Polymers. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-1, -2 |
Lanxess Durethan® B 30 S FN30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, halogen free flame retardant, heat-aging resistanceInformation provided by LANXESS. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | DIN 53461; ASTM D648 |
Kolon Kopa® KN133 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C @Thickness 3.17 mm |
149 °F @Thickness 0.125 in |
un-annealed; ISO 75 |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | |
LATI Latilub 62-10T PA6 Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | |
LATI Latilub 66-02S PA66, Silicone Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Noryl V180HF PPE+HIPS (Europe-Africa-Middle East) NORYL V180HF is an unfilled, flame retardant material. It has been fully optimized w.r.t. flow and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
A. Schulman POLYFORT™ FTP 3130H-01/FTP 3130HU-Colors DescriptionPolyfort® FTP 3130H-01 (non-UV stabilized) and FTP 3130HU-Colors (UV-stabilized) are high flow injection molding polyolefin alloys which exhibit an exceptional stiffness-impact balance a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-2 |
Borealis Borstar® MB7542 High Density Polyethylene for Injection Molding Borstar MB7541 is a bimodal, natural, high density polyethylene produced by the Borstar PE technology. Borstar MB7541 combines excellent organoleptic properties, Environmental Stress Crack Resistan.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
Eastman DuraStar DS1110UVI Polymer, Natural Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-1/-2 |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | dry; ISO 75-1/-2 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648, ISO 75 |
EPICHEM Epinyl PA 6 Polyamide 6 Characteristics: medium viscosity, good mechanical properties |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Af |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM Test |
BASF Ultramid® 8202 HS PA6 (Dry) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-2 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75 |
BASF Ultramid® B27 E 01 PA6 (Dry) Ultramid B27 E 01 is a low viscosity general-purpose, extrusion PA6 grade well suited for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | ISO 75-2/A |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |