Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.03 g/cm³; DIN 53479 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
ISO 527-2/50 |
Elongation at Yield | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
ISO 527-2/50 |
Tensile Modulus | 3.00 GPa @Temperature 23.0 °C |
435 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
Charpy Impact Unnotched | 8.70 J/cm² @Temperature 23.0 °C |
41.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 223 °C | 433 °F | ISO 3146 |
Maximum Service Temperature, Air | 75.0 °C | 167 °F | Continuous (GTP 50% Tensile); IEC 60216 |
175 °C | 347 °F | Short Time; IEC 60216 | |
Deflection Temperature at 0.46 MPa (66 psi) | 170 °C | 338 °F | Unannealed; ISO 75-2/B |
Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | Unannealed; ISO 75-2/A |
Flammability, UL94 | V-2 @Thickness 0.800 mm |
V-2 @Thickness 0.0315 in |
ALL; UL 94 |
V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
UL 94 | |
V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
UL 94 | |
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Flammability Index; IEC 60695-2-12 |
850 °C @Thickness 1.60 mm |
1560 °F @Thickness 0.0630 in |
Flammability Index; IEC 60695-2-12 | |
850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Flammability Index; IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
Descriptive Properties | Value | Comments |
---|---|---|
Additive | Flame Retardant | |
Forms | Pellets | |
Generic Material | Nylon 6 | |
Generic Name | Polyamide 6 (Nylon 6) | |
Processing Method | Injection Molding | |
Regional Availability | Africa & Middle East | |
Asia Pacific | ||
Europe | ||
RoHS Compliance | RoHS Compliant |