Polymer Property : Deflection Temperature at 8.0 MPa = 122 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:3
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Deflection Temperature at 8.0 MPa 50.0 - 204 °C
122 - 399 °F
Average value: 141 °C Grade Count:20
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® A 30 H2.0 901510 Nylon 66
PA 66 standard injection molding grade, non-reinforced, very easy release, good heat-ageing resistanceApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® B 31 SK 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, easy flow, easy-release, rapid solidification, crystallizes somewhat more finely and uniformly than B 30 S
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® DP 1100/30 H2.0 901510 Nylon 6, Micro Glass Balls
PA6, molding grade, micro glass balls, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® DP 2325 H3.0 000000 Nylon 66
PA 66, injection molding grade, non-reinforced, elastomer-modified, good heat-ageing resistance, extremely high notched impact strength even at dry state and at low temperatures
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6
PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Pocan® B 7375 000000 PBT, White Pigment
PBT, 25% white pigments, injection molding, improved light reflection, low tendency to warp
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres
PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® A 30 000000 Nylon 66
PA 66, standard injection molding grade, non-reinforced, very easy release, normal solidificationApplication Examples: terminal blocks, cable clips, bobbins, gearwheels
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral
PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber
PBT, 7% glass fibers, injection molding, flame retardant
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
Lanxess Pocan® DP 1105 000000 PBT
PBT, non-reinforced, injection molding, extrusion, improved flowability
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30
Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr..
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
EMS-Grivory Grivory® BM-30 FR PA6-MD30 FR
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15
Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop..
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSK-30/4 PA666-GB30
Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa..
Deflection Temperature at 8.0 MPa 50.0 °C
122 °F
ISO 75-1/-2
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..