Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 960 °C | 1760 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
Flammability Index; IEC 60695-2-12 |
PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Glow Wire Test | 960 °C | 1760 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 66 GF 30 FRA 5 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Glow Wire Test | 960 °C | 1760 °F | GWFI |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
Flammability Index; IEC 60695-2-12 |
PolyOne Bergamid™ A70 G30 U Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Glow Wire Test | 960 °C | 1760 °F | |
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop. Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCP761 PPE-TPE (Asia Pacific) Flexible Noryl injection molding grade. Low specific gravity with very good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain re.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
Glow Wire Test | 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
IEC 60695-2-12 |
SABIC Innovative Plastics LNP THERMOCOMP PCAF04FRHH PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* PCA04FRHH is a 20 % glass reinforced PC+ABS blend without chlorinated or brominated flame retardants. LNP* THERMOCOMP* complies with the material requirements as specified in TCO'99.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL LTA6020 PPE+PS (Asia Pacific) |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Glow Wire Test | 960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
Glow Wire Test | 960 °C | 1760 °F | UNE 20-672-83 |
PlastxWorld Veroplas PB3301F Nylon 66 flame retarded (UL94 V0), 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Glow Wire Test | 960 °C | 1760 °F | I.E.C. 695-2-1 |
Cossa Polimeri ESTACARB 2060 V0 HF Flame Retardant Polycarbonate Flame retardant class V0, opaque, antimony, chlorine and bromine free, high impact resistance, high thermal resistance, good melt flow rate, good processability, good light resistanceInformation pro.. |
|||
Glow Wire Test | 960 °C | 1760 °F | I.E.C. 695-2-1 |
Cossa Polimeri ESTADIENE 1016 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Eurostar Starflam AFR560B1 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B1 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 60695-2-12 |
Eurostar Starflam RFK517E PA66, Glass/Mineral Fiber Reinforced, Flame Retardant, Injection Molding Starflam RFK517E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filled, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
PN-EN-60695-2-12 |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Glow Wire Test | 960 °C @Thickness 3.20 mm |
1760 °F @Thickness 0.126 in |
IEC 60695-2-12 |
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |