PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF PolyOne OnFlex™ S FR 40A-3S1841 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halogen based flame retardant system. Furthermore, OnFlex™-S FR compounds offer excellent mechanical properties, good elevated temperature compression set performance, very wide hardness range and good processability.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
ISO 868
Tensile Strength at Break 4.50 MPa
653 psi
ISO 37
Tensile Stress 1.10 MPa

@Strain 100 %
160 psi

@Strain 100 %
ISO 37
3.10 MPa

@Strain 300 %
450 psi

@Strain 300 %
ISO 37
Elongation at Break 430 %
430 %
ISO 37
Tear Strength 18.0 kN/m
103 pli
ISO 34-1
Compression Set 14 %

@Temperature 23.0 °C,
Time 259000 sec
14 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
27 %

@Temperature 70.0 °C,
Time 79200 sec
27 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
47 %

@Temperature 100 °C,
Time 79200 sec
47 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
Oxygen Index 27 %
27 %
ISO 4589-2
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
Flammability Index; IEC 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Descriptive Properties Value Comments
Agency Ratings UL QMFZ2 .E76261
Features Flame Retardant
Halogenated
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Business Equipment
Electrical/Electronic Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved