| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Melt Flow | 4.0 g/10 min <br>@Load 10.0 kg,<br> Temperature 250 °C |
4.0 g/10 min <br>@Load 22.0 lb,<br> Temperature 482 °F |
ASTM D1238 |
| Melt Index of Compound | 8.0 g/10 min <br>@Load 5.00 kg,<br> Temperature 280 °C |
8.0 g/10 min <br>@Load 11.0 lb,<br> Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| 20 g/10 min <br>@Load 5.00 kg,<br> Temperature 300 °C |
20 g/10 min <br>@Load 11.0 lb,<br> Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 |
| Tensile Strength, Yield | 71.0 MPa | 10300 psi | 50 mm/min; ISO 527 |
| 72.0 MPa | 10400 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 8.0 % | 8.0 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 4.0 % | 4.0 % | 50 mm/min; ISO 527 |
| 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.68 GPa | 389 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 105 MPa | 15200 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
| 105 MPa | 15200 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.58 GPa | 374 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
| 2.60 GPa | 377 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 2.20 J/cm | 4.12 ft-lb/in | ASTM D256 |
| Izod Impact, Notched (ISO) | 16.0 kJ/m² | 7.61 ft-lb/in² | 80*10*4; ISO 180/1A |
| 8.00 kJ/m² <br>@Temperature -30.0 °C |
3.81 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| 8.00 kJ/m² <br>@Temperature -40.0 °C |
3.81 ft-lb/in² <br>@Temperature -40.0 °F |
80*10*4; ISO 180/1A | |
| 10.0 kJ/m² <br>@Temperature -20.0 °C |
4.76 ft-lb/in² <br>@Temperature -4.00 °F |
80*10*4; ISO 180/1A | |
| 11.0 kJ/m² <br>@Temperature -10.0 °C |
5.23 ft-lb/in² <br>@Temperature 14.0 °F |
80*10*4; ISO 180/1A | |
| 12.0 kJ/m² <br>@Temperature 0.000 °C |
5.71 ft-lb/in² <br>@Temperature 32.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/2C |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | 277 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| Deflection Temperature at 1.8 MPa (264 psi) | 123 °C | 253 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 126 °C <br>@Thickness 6.40 mm |
259 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 144 °C | 291 °F | Rate B/120; ISO 306 |
| 155 °C | 311 °F | Rate A/120; ISO 306 | |
| Flammability, UL94 | V-1 <br>@Thickness 1.00 mm |
V-1 <br>@Thickness 0.0394 in |
UL 94 |
| V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
UL 94 | |
| 5VA <br>@Thickness 2.50 mm |
5VA <br>@Thickness 0.0984 in |
UL 94 | |
| Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 825 °C | 1520 °F | IEC 60695-2-13 | |
| 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 250 - 400 V | 250 - 400 V | UL 746A |