Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combinesThis data was supplied by SABIC-IP f.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non brominated flame retardant with metallic or pearlescent appearance. MAGIX color package may affect performance.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
PTS PCA-2010 Flame Retardant PC/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Asia Pacific) 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS High impact and ductility at 73F (23C) and -20F (-29C). |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
Ineos ABS Lustran® 1148 General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.60 mm |
140 °F @Thickness 0.0630 in |
UL746B |
Ineos ABS Lustran® QE 1094 AS General Purpose, High-Impact
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
LG Chemical AF360C ABS, TBBA-free Flame Retardant, High Flow Feature: Injection Molding, TBBA-free Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9 and 1309-64-4Information provided by.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.60 - 1.70 mm |
140 °F @Thickness 0.0630 - 0.0669 in |
|
LG Chemical LUPOY EC5000AF PC/ABS, Flame Residence Description: Injection Molding, PC/ABS, Flame Residence, Anti-StaticApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 68928-70-1Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.70 mm |
140 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
LG Chemical SG175 ABS, Super Surface Gloss Feature: Injection Molding, Super Surface GlossApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
|
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
UL RTI, Mechanical with Impact | 60.0 - 80.0 °C | 140 - 176 °F | Average value: 63.3 °C Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |