Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746 |
PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | Minimum thickness 0.058 inches. |
LyondellBasell Pro-fax 7624 Polypropylene Impact Copolymer, Heat- and Extraction-Resistant Primary Processing Method: Injection MoldingKey Features: resistant to aging at high temperatures in both wet and dry environments, good cold impact resistance, excellent dimensional stability, FDA .. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | Minimum thickness 0.038 inches. |
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer Key Features: excellent cold impact resistance, good stiffness and impact balance, FDA acceptableApplications: automotive parts, luggage, totes, bins, carrying cases, appliancesMeets FDA requirement.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL746B |
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL RN1300 PPE (Asia Pacific) 15% glass/mineral reinforced PPE. Nonchlorinated, nonbrominated, flame-retardant. Black and gray. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1 PPE+HIPS (Europe-Africa-Middle East) NORYL SE1 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL SE1 is V1 at 1.47 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2212EPR PEI 20% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA lising. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5311 PEI 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific) Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East) LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746 |
Styron EMERGEâ„¢ 4702-15 Polycarbonate EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746 |
Styron EMERGEâ„¢ 4850-19 Polycarbonate EMERGEâ„¢ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL EN265 PPE+PS Extrusion grade. 254F (123C) DTUL. UL94 V-1 rated. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product for Film |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
UL RTI, Mechanical with Impact | 105 °C | 221 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |