Polymer Property : UL RTI, Electrical = 50.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 50.0 °C
122 °F
UL 746
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics GELOY HRA150 ASA (Europe-Africa-Middle East)
GELOY HRA150 is a high heat resistant ASA+PC. GELOY HRA150 shows high impact retention and color stability upon weathering, and hence can be positioned in various outdoor and indoor applications req..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics Lexan® FL3000 PC
Structural foam: 10% weight reduction at 0.250" wall with non-brominated and non-chlorinated FR systems. Impact modified PC with excellent low-temperature impact and UV-stability.This data was supp..
UL RTI, Electrical 50.0 °C
122 °F
UL 746
PolyOne Geon™ 80510 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
UL RTI, Electrical 50.0 °C
122 °F
UL 746
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
UL RTI, Electrical 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:4
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
UL RTI, Electrical 50.0 °C
122 °F
Average value: 50.0 °C Grade Count:5
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
UL RTI, Electrical 50.0 °C

@Thickness 1.57 - 6.33 mm
122 °F

@Thickness 0.0618 - 0.249 in
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet
High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics Noryl PX5622 PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL SPN420 PPE+PS (Asia Pacific)
Superior Productivity plus heat and impact resistance. Excellent processability.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL V01525 PPE+HIPS
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP LUBRICOMP Noryl_SPN422L PPE+PS
LNP* Lubricomp* Noryl_SPN422L compound is a wear resistant, fluorocarbon alloy, 235F (113C) HDT. UL94 HB rated. Check surface aesthetics prior to material specification.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC202M PPE+PS
DATA ON BK1005 ONLY.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC3008A PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_HMC3008A compound is a 30% glass/mineral/carbon fiber reinforced resin; static dissipative; 250F (120C) HDT. Tight tolerance molding.
UL RTI, Electrical 50.0 °C

@Thickness 3.00 mm
122 °F

@Thickness 0.118 in
UL 746
Teknor Apex APEX® 6500-105 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Extrusion Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Compon..
UL RTI, Electrical 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde..
UL RTI, Electrical 50.0 °C
122 °F
Teknor Apex Elexar® EL 1934E Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl GFN3 is a standard 30 % glass filled material with a HDT/A of 145C according to ISO 75
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific)
Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL PX1265 PPE+PS (Asia Pacific)
Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL PX1390 PPE+PS
Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL.
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS
LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray.
UL RTI, Electrical 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
Teknor Apex APEX® 7500-90 Polyvinyl Chloride, Flexible
Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL..
UL RTI, Electrical 50.0 °C
122 °F
UL-746B
Axiall Suprel® SVA 9420 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies ..
UL RTI, Electrical 50.0 °C
122 °F
UL-746B
Axiall Suprel® SVA 9812 Rigid PVC, Extrusion
Georgia Gulf Suprel® SVA 9812 Alloy is an extrusion grade thermoplastic designed for sheet or profile applications requiring high impact resistance. Key features of Suprel 9812 alloy are flame ret..
UL RTI, Electrical 50.0 °C
122 °F
UL-746B
Axiall Suprel® SVA 9301 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9301 is a general purpose injection molding alloy with mid-range properties, providing a balance of impact strength and stiffness and featuring excellent UL flammability li..
UL RTI, Electrical 50.0 °C
122 °F
UL 746B
SABIC Innovative Plastics NORYL EN185 PPE+PS
Extrusion grade. Excellent impact strength. 185F (85C) DTUL. UL94 V-1 rated.