Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
Nylene® PA6/6 Homopolymer 134 HSL Nylon 6/6 Low Viscosity Nucleated Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ensinger ENSILON® 6/6 Extruded Nylon 6/6 (PA66)
(discontinued **) ENSILON materials have high mechanical strength and superior resistance to wear and organic chemicals.Ensilon grades have been replaced by Tecamid.Information supplied by Ensinger, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Kolon KOPA® KN3322V0Y Flame Retardant Nylon 66 Halogen free, Impact -resistantApplications A variety of connectorsInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET) Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
LATI Latamid 66 H2 G/25-V0CT4 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Lat.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP UAL23AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UAL23AS is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include : Internally Lubricated, Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOTUF VF004S PA 66 LNP THERMOTUF* VF004S is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ISO 75 |
Polyram PlusTek PA351M8 Nylon 6.6 for Injection Molding, 40% Mineral Reinforced 40% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | 0.455 MPa |
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Unitika UNILATE® 1 SC PET Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DIN 53461 |
Polyram PlusTek RA103 Nylon 6.6, Impact Modified Impact resistant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ensinger Tecamid® 6/6 Nylon (PA66) Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)Information provided by Ensinger, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol BR2029 Nylon 66, General Purpose, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol PA111 Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Clariant Renol PA11BK FDA Nylon 66, General Purpose, FDA, Black Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Starflam AFR662B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR662B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LS Nylon 66 A general purpose Nylon 66, lubricated and heat stabilized for injection molding.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Ashley Polymers Ashlene® 528LW Nylon 66 General purpose injection molding grade.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Cheng Yu Plastic E2315 Flame Retardant PET, 15% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | ASTM D648 |
Toyobo Vylopet® EMC120K Glass Reinforced Polyester, Easy Molding Grade Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trackin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 235 °C | 455 °F | |
LATI Latilub 66-01M PA66, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |