Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
SABIC PP 5707N Polypropylene Homopolymer STIFFPACT for Injection Molding Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
SABIC PS 126 General Purpose Polystyrene for Injection Molding Product Description: General purpose Polystyrene PS 125 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Network Polymers NPP 25-0802 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 4 mm thick;10.0 mm wide molded rod; ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® ESD 7300 PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for inj.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO 75/Method Bf |
Premix Thermoplastics PRE-ELEC® PP 1370 PRE-ELEC PP 1370 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 100 °C | 194 - 212 °F | ISO 75-2 |
Prodways PLASTCure Model 200 3D Printing Polymer High temperature resistance.Thermoforming applicationsInformation provided by Genistar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® CY201 PC+ABS (Europe-Africa-Middle East) Cycoloy* CY201 is an industrial quality PC+ABS Flame Retardant grade for injection moulding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs F30 ABS Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
Ineos ABS NOVODUR® L3FR ABS, Injection Grade
(discontinued **) Injection molding grade, flame retardant, very easy flow. Contains no polyhalogenated diphenyls or diphenyl ethers.Applications: Television and computer housings.Information provided by the manufact.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer Primary Processing Method: Injection MoldingKey Features: good cold impact resistance, good stiffness and impact balance, excellent dimensional stability, FDA acceptableApplications: seating, applia.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 2-9301 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9301 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9301 is developed for produ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO 75-1,-2 |
Inno-Comp INNOPOL® CS 3-8000 FR Flame Retardant Polypropylene Blend INNOPOL® CS 3-8000 FR is a flame retarded polypropylene compound based on a specific blend of polypropylene homo polymer and copolymer. This grade is available in natural and custom colored form... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
JPJ Technologies PP H35S Homopolymer for Injection Molding PP H35S is specifically developed for producing injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products. Application: General u.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Halar® 930LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Spartech Plasticor Fluted PP Co/Pol Corrugated Sheet Description: Corrugated SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO 75 |
Styrolution PS 2710 HIPS Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® NH-1001T PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PC180X PPE+PS Nonbrominated, nonchlorinated flame retardant. V-1/5VA rated; 175F (90C) HDT. Improved productivity and reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 984 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 984 is a medium impact polypropylene used primarily for automotive parts subjected to impact.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO 75 |
Polyram RamLloy PBB503 PC/ABS Alloy, Flame Retardant and Heat Stabilized Flame retardant and heat stabilized PC/ABS alloy for injection molding applications.Information provided by Polyram. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Eastman Tenite 371A2R30008 Cellulose Acetate Propionate, Natural, Trsp Applications:Consumer-Personal CareToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, c.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ISO R75 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
Aclo Accucomp ABS ABS827L Electroplating Grade |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | |
BASF Procom® D 1118 Polypropylene Data was collected by ISO methods and provided by BASF. |