Material Notes:
Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability, god flow properties for excellent part filling, high stiffness and good clarity in the products. This grade allows for short cycle times.Typical Applications: PP 5707N can be used for housewares thin wall packaging, caps & closures and garden furniture items with good dimensional stability.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 - 0.025 cm/cm
0.012 - 0.025 in/in
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 1800 MPa
261000 psi
ASTM D790A
Izod Impact, Notched 0.330 J/cm
0.618 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525B
Processing Properties Metric English Comments
Processing Temperature 200 - 235 °C
392 - 455 °F
Barrel Temperature
Mold Temperature 15.0 - 40.0 °C
59.0 - 104 °F