Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific) Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | unannealed; ASTM D648 |
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 - 122 °C | 196 - 252 °F | Average value: 105 °C Grade Count:84 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | |
Ineos ABS Centrex® 833 ASA+AES Blend
(discontinued **) Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ASTM D648 |
Flint Hills P9H9Z-018 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical PI641 ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ISO 75B |
Lucite International Diakon® CLG356 Acrylic Polymer Information provided by Lucite International |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ISO 75B |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ASTM D648 |
Flint Hills P5M6N-058A Polypropylene Random Copolymer Features: Excellent processabilty, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: consumer disposable itemsInformation .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | |
Ineos ABS Triax® 1120 ABS + Polyamide Blend (DAM) Key Features:UnfilledPlatableHigh impact or high impact modifiedSuitable processing methods:Injection moldingFilm extrusionBlow molding |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics PREVEX VGAX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 3.20 mm |
196 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Asia Pacific) LNP STAT-LOY A3000 is a compound based on Acrylonitrile butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistatic. Also known as: STAT-LOY A |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific) LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ISO 75 |
Teijin Multilon TN-7500 Halogen-Free Flame Resistant PC/ABS Polymer Alloy Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has excellently high flowability, i.e., suitable for a large-scale business machine chassis.Information provided by T.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ISO 75-2 |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | ASTM D648 |
Ashley Polymers Ashlene® ABS 243 Medium impact, high flow, rigid. Suitable for injection molding of appliances, automotive components, office machines, switch boxes and panels.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C @Thickness 6.40 mm |
196 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | |
Eastman Tenite 383A-12 CAP Cellulose Acetate Propionate
(discontinued **) 12% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 °C | 196 °F | |
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate