Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYelast TPE EC90 D50 P05B Thermoplastic Elastomer, PP/EPDM Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Geloy XTWM200 ASA ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 484C High Impact Polystyrene
(discontinued **) STYRON® 484C high impact polystyrene resin, is typically used in refrigeration applications, appliances, containers, lids, furniture and profiles. It offers excellent low temperature toughness, exc.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® XL-8028 High Impact Polystyrene
(discontinued **) STYRON® XL-8028 high impact polystyrene is designed for VCR cassettes, toys, small appliances, telephones, housewares, tool items, computer consoles and bodies for computer cartridges. It offers hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 3.20 mm |
189 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics GELOY CR7520 ASA General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | |
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa FW-650 Flame Retardant ABS Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Ineos J60-800-178 HDPE A high density polyethylene homopolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still and sparkling water.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Ineos T60-500 HDPE T60-500 is a high density polyethylene homopolymer designed specifically for injection molding. This narrow molecular weight distribution resin is a product of Ineos USA, LLC's innovative technolog.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
LyondellBasell Astryn NXO-21001 Polypropylene Copolymer Key Features: high melt flow, medium modulus polypropylene copolymer, high flow, excellent processability, excellent colorabilityApplications: wire harnesses, housings, thin walled partsDescription:.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C @Thickness 6.40 mm |
189 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-2 |
Borealis Daplen™ EE115AE TPO Compound Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | 0.125 inch; ASTM D648 |
PlastxWorld CEVIAN®-V 500 ABS Medium Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-1/-2 |
Covestro Bayblend® FR 3005 Polycarbonate + ABS, Flame Retardant Grade Injection molding gradeeasy-flow gradeVicat/B 120 temperature = 95 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (2.0 mm)no j.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | dry; ISO 75-1/-2 |
DSM Novamid® ST220 NAT PA6-I Impact Modified, Injection Molding, Medium Viscosity |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | Unannealed; ASTM Data |
Dow Retain® ABS 7342 ABS Data provided by Dow Chemical. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® 6646 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 66 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D-648 |
Bapolan® 6409 Polystyrene, Injection Grade Bapolan PS6409 is designed for injection molding applications requiring superior impact and gloss. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Application: General purpose.Bapolene® a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Bapolene® PP5010 Polypropylene, Extrusion Grade Bapolene PP5010 is an extrusion PP high impact copolymer with excellent color and processability. It offers extra high impact strength and low temperature properties.Applications: Auto, pipe, profi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | |
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Eastman Tenite Butyrate 465E2R30008 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Eastman Tenite Butyrate 513E3720012 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 87.0 °C | 189 °F | ASTM D648 |
Samyang Triel® 5500 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5500 is an extrusion grade.Information provided by Samyang. |