Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9333G is a 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface a..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with..
CTE, linear, Transverse to Flow 84.0 - 120 µm/m-°C
46.7 - 66.7 µin/in-°F
Average value: 103 µm/m-°C Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
CTE, linear, Transverse to Flow 84.0 - 110 µm/m-°C

@Temperature 23.0 °C
46.7 - 61.1 µin/in-°F

@Temperature 73.4 °F
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP
LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant...
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RFL46ES PA 66
LNP* LUBRICOMP* RFL46ES is a compound based on Nylon 6/6 containing 30% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Heat Stabilized, Easy Molding.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRILOY UX99725 PPA
LNP LUBRILOY* UX99725 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP MX95318 PP
LNP* THERMOCOMP* MX95318 is a compound based on Polypropylene containing Proprietary Filler(s).
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66
LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp RF006PS PA 66
LNP* Thermocomp* RF-1006 EP HS is based on Nylon 6/6 containing Glass Fiber. Characteristics of this grade include Exceptional Processing and Heat Stabilizer.This data was supplied by SABIC-IP for ..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF00ASXS PA6.6 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00ASXS is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RFB53XXZ PA 66
LNP* THERMOCOMP* RFB53XXZ is a compound based on Nylon 66 resin containing 15% Glass Fiber, 25% Glass Bead.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66
LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 200 °C
46.7 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 200 °C
46.7 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 200 °C
46.7 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 200 °C
46.7 µin/in-°F

@Temperature 73.4 - 392 °F
ASTM D696
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue
Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 55.0 - 160 °C
46.7 µin/in-°F

@Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)  (Unverified Data**)
40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 84.0 µm/m-°C
46.7 µin/in-°F
ISO 11359
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of st..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance ..
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP CL002 PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* CL002 is a compound based on Polystyrene resin containing PTFE. Added features include: Internally Lubricated.
Copyright © lookpolymers.com All Rights Reserved