Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® MC1300 PC+ABS (Asia Pacific) Cycoloy MC1300 resin is an injection moldable PC/ABS blend featuring excellent flow and impact performance. It is designed for plating applications mostly used in automotive industry. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 3300SGH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics, low flash and rapid cure. This compound i.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BKV 130 GIT DUS008 900116 Nylon 6, Impact Modified PA 6, 30% glass fibers, injection molding, impact modified, GIT/WITInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow) |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP BM 410 H2.0 901510 Nylon 6, 10% Mineral + Glass Fiber PA 6, injection molding grade, 10% glass fibers/mineral, good heat-ageing resistance |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KL 1-7265 000000 PBT, 15% Glass Fiber PBT, 15% glass fibers, injection molding |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RA004 is a compound based on Nylon 66 resin containing Aramid Fiber. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
50.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON MD000AP PP LNP* STAT-KON* MD000AP is a compound based on Polypropylene containing Carbon Powder. Added features of this grade include: Electrically Conductive, Exceptional Processing. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PX1005X PPE+HIPS (Europe-Africa-Middle East) Noryl PX1005X is an unfilled, low heat resistance, halogen free (according VDE/DIN 472 part 813) flame retardant material. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 330HR Polybutylene Terephthalate (PBT), Hydrolysis resistant, Heat shock resistant, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K222-D Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7912 MBS151 Polycarbonate + PBT, Impact Grade (PC+PBT)-blendsimpact modifiedInjection molding grademedium flowhigh toughness at low temperaturesideal for painted applicationunreinforcedAs of 1 September 2015, Bayer MaterialScience was separated.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Makroblend® UT5205 PC/PBT Blend Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BM-30/2 PA6-MD30 Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 55 LY PA12/MACMI Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 55 LY offers a variety of interesting properties such as: c.. |
|||
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TS V0 PA666 Product description: Grilon TS V0 is an unreinforced, normal viscosity, self-extinguishing Polyamid 66 + Polyamide 6 injection molding grade. Grilon TS V0 is halogen free and free of red phosphorous.. |