Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.50 g/cc | 0.0542 lb/in³ | DAM; ISO 1183 |
Water Absorption | 5.0 % @Thickness 2.00 mm |
5.0 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
Moisture Absorption | 1.60 % @Thickness 2.00 mm |
1.60 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
Linear Mold Shrinkage, Flow | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 95 | 95 | DAM; ISO 2039-2 |
Hardness, Rockwell R | 121 | 121 | DAM; ISO 2039-2 |
Tensile Strength at Break | 55.0 MPa | 7980 psi | 50%RH; ISO 527-1/-2 |
85.0 MPa | 12300 psi | DAM; ISO 527-1/-2 | |
Elongation at Break | 4.0 % | 4.0 % | DAM; ISO 527-1/-2 |
9.0 % | 9.0 % | 50%RH; ISO 527-1/-2 | |
Tensile Modulus | 3.80 GPa | 551 ksi | 50%RH; ISO 527-1/-2 |
6.60 GPa | 957 ksi | DAM; ISO 527-1/-2 | |
Shear Modulus | 0.427 GPa @Temperature 150 °C |
61.9 ksi @Temperature 302 °F |
DAM; Dynamic; ISO 11403-1 -2 |
0.544 GPa @Temperature 110 °C |
78.9 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
1.226 GPa @Temperature 62.0 °C |
177.8 ksi @Temperature 144 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
2.393 GPa @Temperature 10.0 °C |
347.1 ksi @Temperature 50.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
2.504 GPa @Temperature -20.0 °C |
363.2 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
2.692 GPa @Temperature -50.0 °C |
390.4 ksi @Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
Charpy Impact Unnotched | 3.50 J/cm² | 16.7 ft-lb/in² | DAM; ISO 179/1eU |
5.50 J/cm² | 26.2 ft-lb/in² | 50%RH; ISO 179/1eU | |
2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
Charpy Impact, Notched | 0.350 J/cm² | 1.67 ft-lb/in² | DAM; ISO 179/1eA |
0.400 J/cm² | 1.90 ft-lb/in² | 50%RH; ISO 179/1eA | |
0.200 J/cm² @Temperature -30.0 °C |
0.952 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
Tensile Creep Modulus, 1 hour | 3500 MPa @Time 3600 sec |
508000 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
Tensile Creep Modulus, 1000 hours | 2100 MPa @Time 3.60e+6 sec |
305000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 65.0 µm/m-°C | 36.1 µin/in-°F | DAM; ISO 11359-1/-2 |
CTE, linear, Transverse to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | DAM; ISO 11359-1/-2 |
Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | DAM; ISO 75-1/-2 |
Deflection Temperature at 1.8 MPa (264 psi) | 170 °C | 338 °F | DAM; ISO 75-1/-2 |
Flammability, UL94 | HB @Thickness 0.700 mm |
HB @Thickness 0.0276 in |
DAM; IEC 60695-11-10 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | 50%RH; IEC 60093 |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | 50%RH; IEC 60093 |
Dielectric Constant | 3.9 @Frequency 1.00e+6 Hz |
3.9 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 |
4.5 @Frequency 1.00e+6 Hz |
4.5 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
4.5 @Frequency 100 Hz |
4.5 @Frequency 100 Hz |
DAM; IEC 60250 | |
9.4 @Frequency 100 Hz |
9.4 @Frequency 100 Hz |
50%RH; IEC 60250 | |
Dielectric Strength | 40.0 kV/mm | 1020 kV/in | DAM; IEC 60243-1 |
Dissipation Factor | 0.011 @Frequency 100 Hz |
0.011 @Frequency 100 Hz |
DAM; IEC 60250 |
0.023 @Frequency 1.00e+6 Hz |
0.023 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 | |
0.055 @Frequency 1.00e+6 Hz |
0.055 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
0.21 @Frequency 100 Hz |
0.21 @Frequency 100 Hz |
50%RH; IEC 60250 | |
Comparative Tracking Index | 575 V | 575 V | DAM; IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Part Marking Code | >PA66-MD40< | ISO 11469 |
Regional Availability | Europe | |
Near East/Africa | ||
Resin Identification | PA66-MD40 |