Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
Manufacturer Polyplastics Co.
Trade Name Duranex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastics Duranex® 7307 Polybutylene Terephthalate (PBT), Super low warpage, GF filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers or other inorganic filler additives. Various grades are available, including flame-retardant, reinforced, and impact-resistant grades. DURANEX®, due to its mechanical strength, heat stability, electrical resistivity and wear and abrasion-resistance, offers great potential as a well-balanced, highly reliable material, having a wide variety of applications including electronic / electro-mechanical and automobile parts and various other functional parts. DURANEX® also assures moldability, dimensional stability, glossy surfaces and various fabrication capabilities providing higher added value.Information provided by PolyPlastics.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 106 MPa
15400 psi
ISO 527-1, 2
Elongation at Break 2.8 %
2.8 %
ISO 527-1, 2
Flexural Strength 168 MPa
24400 psi
ISO 178
Flexural Modulus 6.50 GPa
943 ksi
ISO 178
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1, 2
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: