Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East) CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Cycoloy® FXC810SL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require sparkle colour effects with lowered RFI inhibitor. Colour package may effect perform.. |
|||
CTE, linear, Transverse to Flow | 80.0 - 120 µm/m-°C | 44.4 - 66.7 µin/in-°F | Average value: 96.0 µm/m-°C Grade Count:5 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
CTE, linear, Transverse to Flow | 80.0 - 110 µm/m-°C | 44.4 - 61.1 µin/in-°F | Average value: 89.3 µm/m-°C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® B 38 FKA 000000 Nylon 6, Film Grade PA 6 film-grade, medium to higher viscosity, with processing aid and slip agent, nucleated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion fo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® T 7391 POS151 900044 PBT + PET, 45% Glass Fiber PBT + PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load UV stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® BKV 30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, injection molding grade with 30% glass fibers, good heat-ageing resistance |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP BKV 60 H2.0 EF 900116 Nylon 6, 60% Glass Fiber PA 6, injection molding grade, 60% glass fibers, low viscosity, good flowability (Easy Flow), good heat-resistanceApplication Examples: gearbox housings, spring holders, automotive door handles |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® BF 4235 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duranex® 733LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
|
Covestro Baydur® 40 Polyurethane Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 1S XE 4224 nat PA1010 Product Description: Grilamid XE 4224 natural is a heat and UV stabilized high viscosity polyamide 1010 (PA1010), designed for extrusion. In addition the product can be used for thicker injection mo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 1SVX-50H black 9288 PA1010-GF50 Product Description: Grilamid 1SVX-50H black 9288 is a 50% glass fiber reinforced Polyamide 1010 injection molding grade with the following product profile. Key properties of Grilamid 1SBVX-50H LDS .. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2SV-30H black 9992 PA610-GF30 Product Description: GRILAMID XE 3976 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GC-4H PA*-CF40 Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo.. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature 20.0 °C |
44.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Stanyl® TW200F8 (DAM) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
CTE, linear, Transverse to Flow | 80.0 µm/m-°C | 44.4 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® K224-G3-FC NA99001 PA6-GF15 15% Glass Reinforced |