Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Baydur® 40 Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Covestro
Trade Name Baydur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Baydur® 40 Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 0.400 g/cc
0.0145 lb/in³
Water Absorption 0.30 %
0.30 %
Saturation in water
Water Absorption at Saturation 0.30 %
0.30 %
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 11.0 MPa
1600 psi
Elongation at Break 6.0 %
6.0 %
Tensile Modulus 0.440 GPa
63.8 ksi
Charpy Impact Unnotched 0.900 J/cm²
4.28 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistance 2.00e+14 ohm
2.00e+14 ohm
Dielectric Strength 18.0 kV/mm
457 kV/in
Comparative Tracking Index 600 V
600 V
Users viewing this material also viewed the following: