Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Conditioned Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 200 Polyamide 66, Conditioned Application: bearing bushes, machine parts, gears, linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Conditioned Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 309 Cast Polyamide 6, Oil Filled, Dry Application: slippers, inserts for coupling boxes, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2 Filled, Heat Stabilized, Dry Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Dry Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Dry Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Schwartz Technical Plastics LAMIGAMID® 327 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1100 MO Improved sliding and self lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1115 By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | Dry |
Asahi Kasei Leona® 1300S Nylon 66 General purpose grade. Good balance of flowability and mechanical properties.Applications:Connectors, washers, cable ties. Information provided by Asahi Kasei |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | Dry |
Asahi Kasei Leona® 1502 Nylon 66 Similar to 1500 but with improved heat aging resistance.Applications:Under-the-hood automotive parts Information provided by Asahi Kasei |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | Dry |
Asahi Kasei Leona® FR200 Nylon 66 UL94 V-0; halogen-free and phosphor-free.Applications:Connectors, switches, and other electrical and electronic parts Information provided by Asahi Kasei |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | |
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Specific Heat Capacity | 1.67 - 1.67 J/g-°C | 0.399 - 0.400 BTU/lb-°F | Average value: 1.67 J/g-°C Grade Count:17 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Specific Heat Capacity | 1.67 J/g-°C | 0.399 BTU/lb-°F | Average value: 1.67 J/g-°C Grade Count:8 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |