Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-25 Acrylic Resin Extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C @Temperature 100 °C |
0.359 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-30 Acrylic Resin
(discontinued **) Injection molding and extrusion grade pellets. Highest molecular weight and heat resistance of Optix® line with exceptional mold release.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-52 Acrylic Resin
(discontinued **) Injection/extrusion pellets. High heat resistance/medium flow.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-76 Acrylic Resin
(discontinued **) Injection/extrusion pellets. Medium heat resistance with higher flow than PL-52 pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Average value: 1.50 J/g-°C Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe POM Copolymer Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4300 M5 25% Mineral Filled PBT Description: Is a PBT-HI, injection-molding grade reinforced with 25% of minerals, for the production of parts with good surface quality and low warpage, e.g. housings and visible parts of domestic .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Mfr. internal test |
Ascend Performance Materials VYDYNE® R220 Nylon, Mineral Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Conditioned) Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3L BK00464 PA6 (Conditioned) Description: Impact-modified, free-flowing and rapidly processable injection-molding grade for dry impact-resistant technical articles such as, for example, housings, fittings, small parts and wall .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |