Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation properties.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.35 %
0.35 %
DIN 53 495
Mechanical Properties Metric English Comments
Elongation at Break 3.0 %
3.0 %
DIN 53 455
Tensile Modulus 10.0 GPa
1450 ksi
DIN 53 457
Charpy Impact, Notched 3.50 J/cm²
16.7 ft-lb/in²
DIN 53 453
Coefficient of Friction, Dynamic 0.24
0.24
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 130
130
in MPa; DIN 53 455
Thermal Properties Metric English Comments
CTE, linear 20.0 - 30.0 µm/m-°C
11.1 - 16.7 µin/in-°F
Specific Heat Capacity 1.50 J/g-°C
0.359 BTU/lb-°F
Melting Point 225 °C
437 °F
DIN 53 736
Maximum Service Temperature, Air 120 °C
248 °F
Continuous use
190 °C
374 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 22.0 °C
71.6 °F
dynamic; DIN 53 736
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
DIN 53 482
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 50.0 kV/mm
1270 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.0090

@Frequency 1.00e+6 Hz
0.0090

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Creep Resistance Grade CTI 400
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds not resistant
Users viewing this material also viewed the following: