Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 353MA® High Temperature Austenitic Stainless Steel Alloy with higher nickel content than the other steels. Has increased silicon and nitrogen contents and is microalloyed with rare earth metals (REM). Max service temperature in air is 1150°C, but.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 4565 High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | RT |
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Plansee Chromium, Cr; Sintered Characteristics:High corrosion resistanceHigh wear resistanceBeautiful opticsLower melting point than other refractory metalsVery high vapor pressureLower density than other refractory metalsPossess.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 °C |
0.108 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 °C |
0.108 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® B28 High Nickel Super-Austenitic Stainless Steel Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for sp.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 °C |
0.108 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54 Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainl.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals BRIGHTRAY® Alloy F Electrical Resistance Alloy A nickel-iron-chromium electrical-resistance alloy for use at temperatures up to 1920°F (1050°C) under continuous operating conditions. Its high iron content and relatively low level of nicke.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 100 °C |
0.108 BTU/lb-°F @Temperature 212 °F |
|
Special Metals INCOLOY® alloy 028 Austenitic Stainless Steel INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybd.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.75 in.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm) Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.5 x 2.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 355 Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 500 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 500 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 - 0.490 J/g-°C | 0.108 - 0.117 BTU/lb-°F | after modified H900 heat treatment |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ATI Allegheny Ludlum Type 317 Stainless Steel, UNS S31700 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ATI Allegheny Ludlum Type 316L Stainless Steel, UNS S31603 This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels .. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 460 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C | 0.108 BTU/lb-°F | |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 °C |
0.108 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |