Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel

Category Metal , Ferrous Metal , Duplex , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chromium. This alloy presents higher mechanical and corrosion resistance properties than duplex 22 Cr stainless steels. Its yield strength is about twice that of standard austenitic grades and well in excess of that of nitrogen alloyed austenitics. Operation temperature of UR 45 N+ is generally limited from -50°C to 280°C (- 58°F to 536°F). Lower temperature used particularly for welded structures may also be considered, but needs technical background.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 720 MPa
>= 104000 psi
Tensile Strength, Yield >= 510 MPa

@Strain 0.200 %
>= 74000 psi

@Strain 0.200 %
>= 540 MPa

@Strain 1.00 %
>= 78300 psi

@Strain 1.00 %
Elongation at Break >= 25 %
>= 25 %
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.333
0.333
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 90.0 J
>= 66.4 ft-lb
120 J
88.5 ft-lb
Typical
>= 75.0 J

@Temperature -50.0 °C
>= 55.3 ft-lb

@Temperature -58.0 °F
90.0 J

@Temperature -50.0 °C
66.4 ft-lb

@Temperature -58.0 °F
Typical
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 20.0 - 100 °C
6.67 µin/in-°F

@Temperature 68.0 - 212 °F
12.5 µm/m-°C

@Temperature 20.0 - 200 °C
6.94 µin/in-°F

@Temperature 68.0 - 392 °F
13.0 µm/m-°C

@Temperature 20.0 - 300 °C
7.22 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 °C
0.108 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 17.0 W/m-K

@Temperature 20.0 °C
118 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.020 %
0.020 %
Chromium, Cr 22.6 %
22.6 %
Iron, Fe 67.799 %
67.799 %
As remainder
Molybdenum, Mo 3.4 %
3.4 %
Nickel, Ni 6.0 %
6.0 %
Nitrogen, N 0.18 %
0.18 %
Sulfur, S 0.0010 %
0.0010 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000800 ohm-cm

@Temperature 20.0 °C
0.0000800 ohm-cm

@Temperature 68.0 °F