Material Notes:
Description: URANUS® B28 (UR B28) is a super-austenitic stainless steel with very high nickel (31%) and chromium (27%) contents. The molybdenum content is about 3.5%. The alloy is designed for specific purposes, including sulphuric or phosphoric acid applications. It behaves particularly well in sulphuric and phosphoric acid environments, even when contaminated by chlorides and fluorides species. The high nickel content improves its stress corrosion cracking resistance. The combined chromium and molybdenum additions contribute to increase the localized corrosion resistance. The alloy behaves much better than alloy 825 and could be considered in some applications (sour gas) to replace the more expensive 625 grade. The alloy is extensively used in chemical and offshore applications including very sour gas fields.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 250 - 310
250 - 310
Typical, V<sub>10</sub>
Tensile Strength, Ultimate >= 500 MPa
>= 72500 psi
Minimum Guaranteed
Tensile Strength, Yield >= 220 MPa

@Strain 0.200 %
>= 31900 psi

@Strain 0.200 %
>= 250 MPa

@Strain 1.00 %
>= 36300 psi

@Strain 1.00 %
Elongation at Break >= 40 %
>= 40 %
Modulus of Elasticity 195 GPa
28300 ksi
Poissons Ratio 0.30
0.30
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 100 J

@Temperature -196 °C
>= 73.8 ft-lb

@Temperature -321 °F
Thermal Properties Metric English Comments
CTE, linear 15.8 µm/m-°C

@Temperature 20.0 - 200 °C
8.78 µin/in-°F

@Temperature 68.0 - 392 °F
16.5 µm/m-°C

@Temperature 20.0 - 300 °C
9.17 µin/in-°F

@Temperature 68.0 - 572 °F
17.3 µm/m-°C

@Temperature 20.0 - 500 °C
9.61 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 °C
0.108 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 12.0 W/m-K

@Temperature 20.0 °C
83.3 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.020 %
<= 0.020 %
Chromium, Cr 27 %
27 %
Copper, Cu 1.0 %
1.0 %
Iron, Fe 37.43 - 37.45 %
37.43 - 37.45 %
As remainder
Molybdenum, Mo 3.5 %
3.5 %
Nickel, Ni 31 %
31 %
Nitrogen, N 0.050 %
0.050 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000100 ohm-cm

@Temperature 20.0 °C
0.000100 ohm-cm

@Temperature 68.0 °F