Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54

Category Metal , Ferrous Metal , Austenitic , Stainless Steel , T S30000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name URANUS®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel URANUS® B66 High Strength Super-Austenitic Stainless Steel with PREN = 54.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Research carried out these last five years has shown that combined additions of chromium, tungsten, molybdenum, nitrogen and copper, make it possible to design a super-austenitic stainless steel with mechanical properties equivalent to the alloy 625 and with very high corrosion resistance properties. Due to 22% Ni and 0.4% N additions, the new URANUS® B66 (UR B66) alloy exhibits a very stable microstructure, less prone to intermetallic phase precipitations than the other highly alloyed austenitic stainless steels. The UR B66 alloy has improved corrosion resistance properties compared to 6 Mo grades particularly in sea water and chlorinated sea water. Due to the optimum "cocktail" of alloying elements, the grade can be used in most very severe corrosive environments where it behaves almost equivalent or better than alloy 625.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 8.20 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 220 - 260
220 - 260
Typical, V<sub>10</sub>
Tensile Strength, Ultimate >= 750 MPa
>= 109000 psi
Minimum Guaranteed
Tensile Strength, Yield >= 420 MPa

@Strain 0.200 %
>= 60900 psi

@Strain 0.200 %
>= 440 MPa

@Strain 1.00 %
>= 63800 psi

@Strain 1.00 %
Elongation at Break >= 50 %
>= 50 %
Modulus of Elasticity 195 GPa
28300 ksi
Poissons Ratio 0.30
0.30
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Charpy Impact >= 100 J

@Temperature -196 °C
>= 73.8 ft-lb

@Temperature -321 °F
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 - 100 °C
8.33 µin/in-°F

@Temperature 68.0 - 212 °F
16.0 µm/m-°C

@Temperature 20.0 - 300 °C
8.89 µin/in-°F

@Temperature 68.0 - 572 °F
16.5 µm/m-°C

@Temperature 20.0 - 500 °C
9.17 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.450 J/g-°C

@Temperature 20.0 °C
0.108 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 12.0 W/m-K

@Temperature 20.0 °C
83.3 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Chromium, Cr 24 %
24 %
Copper, Cu 1.5 %
1.5 %
Iron, Fe <= 41.1 %
<= 41.1 %
As remainder
Manganese, Mn 3.0 %
3.0 %
Molybdenum, Mo 6.0 %
6.0 %
Nickel, Ni 22 %
22 %
Nitrogen, N >= 0.40 %
>= 0.40 %
Tungsten, W 2.0 %
2.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000100 ohm-cm

@Temperature 20.0 °C
0.000100 ohm-cm

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved