Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 262 °C | 504 °F | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Melting Point | 262 °C | 504 °F | |
Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94.. |
|||
Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66
(Unverified Data**) Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 262 °C | 504 °F | DAM; ASTM D3418 |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Melting Point | 262 °C | 504 °F | ISO 11357-1,-3 |
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers PA 66, 30% glass fibers, injection molding, heat-ageing stabilized |
|||
Melting Point | 262 °C | 504 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:.. |
|||
Melting Point | 262 °C | 504 °F | |
Techmer ES HiFill® PA6/6 GF33 5105 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357 |
Solvay TECHNYL® 2412GHF6 PA66, 33% glass fiber, DRY Description: Polyamid 66, reinforced with 33% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF6 is used in all sectors of indu.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357 |
Solvay TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY Description: Polyamid 66, reinforced with 38% of glass fiber and mineral filler, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2412GM05-D is used in all sectors o.. |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 70G33L BK031 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L BK031 is a 33% glass fiber reinforced black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 70G43HSLA BK099 Nylon 66
(Unverified Data**) 43% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G43HSLA BK099 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® EFE8089B BK416 Nylon 66 Zytel® EFE8089B BK416 is a 33% fiber reinforced, heat stabilized, lubricated, toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FG133F1 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact Applications Zytel FG133F1 NC010 is a nucleated PA 66. It has been developed for consideration into applications such as parts for the food .. |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Melting Point | 262 °C | 504 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NA40 GR25 NL XA 42 PA 6.6 25% glass fiber reinforced, UL94 V0, red phosphorus Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 262 °C | 504 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NA40 GR40 NL PA 6.6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NA40 MF40 BK001 HS PA6.6, 40% mineral filled, heat stabilized, black Information provided by Eurotec® |
|||
Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NA40 MR15 NL IL PA6.6, 15% mineral filled, impact modified, natural Information provided by Eurotec® |
|||
Melting Point | 262 °C | 504 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Melting Point | 262 °C | 504 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NA40 NL IL PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357-1/3 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Conditioned, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357-1/3 |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Melting Point | 262 °C | 504 °F | DAM; 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS BKB009 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productiv.. |
|||
Melting Point | 262 °C | 504 °F | 10 K/min; ISO 3146 |
Eurotec® Tecomid® NA40 GR20 NL PA 6.6 20% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Melting Point | 262 °C | 504 °F | ISO 11357 |
Solvay TECHNYL® 2210HS PA66, DRY Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe.. |